Stainless Steel AISI 430
Data sheet
DIN EN 10088-3
Grade 1.4016
The material 1.4016 / AISI 430 is a magnetisable ferritic stainless steel that is suitable for forging and cold forming. Due to its high chromium content of 16-18 %, this stainless steel grade is more corrosion resistant (especially against stress corrosion cracking) than a comparable material with a lower chromium content. Please note that the material 1.4016 / AISI 430 can only be used for welding to a limited extent. The processing possibilities include cold upsetting and bending.
Specifications
EN material number: 1.4016
EN short name: X6Cr17
EN standard: 10088
Microstructure class: ferrite
Comparable standards and designations
AFNOR Z8C17 *
AISI 430 *
B.S. 430S17 *
JIS SUS430 *
UNS S43000 *
SIS 2320 *
(* in accordance with)
Chemical composition of stainless steel 1.4016
C | Si | Mn | P | S | N | Cr | Cu | Mo | Ni | Ti |
---|---|---|---|---|---|---|---|---|---|---|
≤ 0,08 | ≤ 1,00 | ≤ 0,04 | ≤ 0,04 | ≤ 0,03 | - | 16,0 - 18,0 | - | - | - | - |
Mass fraction in % according to DIN EN 10088-3
Physical properties
Magnetizability: present
Density (kg/dm³): 7.7
Thermal conductivity (at up to 20°C): 25
Electronic resistance at room temperature (in Ω mm²/m): 0.60
Possible areas of application
Automotive industry
Construction industry
Household appliances
Interior design
Food industry
Mechanical engineering
and more
Heat treatment and hot forming
Welding
Hot forging: 800-1100 °C
Soft annealing: 750-850°C
The material 1.4016 / AISI 430 has medium weldability. It is suitable for TIG welding and laser beam welding, but cannot be used for arc welding.
Please note
The information given in this data sheet has been compiled to the best of our knowledge and is based on the current version of the relevant standard. It is considered for reference only and we assume no liability for any errors.
Link to stainless steel wire
Do you have questions about our products?
Please contact us at +49 2263 / 9240-0 or via email info@agst.de